GH3230 Nickel-Based Superalloy Powder 15-53μm for SLM Additive Manufacturing 3D Printing
Price varies depending on material, logo, quantity and customization requirements.
Introduction
| Application | Brazing;Class molds;Forging Heads,etc | Alloy Grade | Inconel 625,718,738,Hastelloy C276,NiCrBSi |
| Purity | ≥99.5% | Particle Size | 15-45 μm,15-53 μm,45-106 μm,53-150 μm |
| Particle Shape | Spherical | Apparent Density | 4.2-5.5 g/cm³ |
| Flowability | Hall Flow ≤25 s/50 g | Oxygen Content | ≤300 ppm or ≤1000 ppm |
| Manufacturing Process | Gas Atomized/Plasma Atomized | Application | Thermal Spray Coatings/3D Printing/Laser Cladding/ |
| CAS NO. | 7440-02-0 |
We are a professional manufacturer and supplier, dedicated to maintaining consistent quality and establishing long-term partnerships with clients worldwide.
Our mission is to provide high-quality products and reliable service. We are committed to offering the following advantages:
- Stable production system ensuring consistent quality, dependable supply, and standardized manufacturing management;
- Strict quality control covering material selection, processing, surface finishing, and final packaging;
- Variety of products and specifications to meet diverse project requirements and application scenarios;
- OEM & customization support based on drawings, samples, or specific technical requirements;
- Flexible packaging solutions to ensure safe handling and transportation of products;
- Continuous improvement in products and services to better support customers in different markets.
If you are interested in our products, please feel free to contact us. We look forward to establishing long-term and mutually beneficial cooperation with you.